Brake cooling duct fabrication question


Author
Message
AlpineCoupe
A
Supreme Being (427 reputation)Supreme Being (427 reputation)Supreme Being (427 reputation)Supreme Being (427 reputation)Supreme Being (427 reputation)Supreme Being (427 reputation)Supreme Being (427 reputation)Supreme Being (427 reputation)Supreme Being (427 reputation)
Group: Forum Members
Posts: 45, Visits: 2.1K
Hello all, Im new to the forum and new to making composite parts. I have made a couple of splitter vents for a race car of mine and now am working on brake cooling ducts for the front air dam. 

My question is how to lay up the carbon fiber to ensure a reasonable release from the mold. It currently looks like this:




I was thinking I could lay it up (after sanding and smoothing of course), as is, vacuum bag it, and essentially make it as one piece. But as I read a couple of other posts on this forum I started to second guess myself. Any suggestions from the collective?

Thanks in advance!

  
Reply
AlpineCoupe
A
Supreme Being (427 reputation)Supreme Being (427 reputation)Supreme Being (427 reputation)Supreme Being (427 reputation)Supreme Being (427 reputation)Supreme Being (427 reputation)Supreme Being (427 reputation)Supreme Being (427 reputation)Supreme Being (427 reputation)
Group: Forum Members
Posts: 45, Visits: 2.1K
MarkMK - 10/24/2019 9:22:35 AM
If you're happy with the basic shape, in that it doesn't pose the risk of a mechanical lock, after sanding back the filler/bondo it would probably be best lay a couple of light fibreglass layers over the pattern

Even if well coated with a suitable paint system, filler/bondo is likely to pull away when it comes to creating an initial mould so the fibreglass skin will add some strength. Once the fibreglass has been roughly sanded, a thin skim of filler can then be used to create a surface smooth enough to apply a top coat. 

The pattern coat primer and hi-coat gloss system that EC sells would be ideal, but some other kind of coating that can bond well to the bare pattern and provide a reliable release surface, after flatting and polishing, depending upon what's available where you are will also work

This will give you a female mould from which you can then create your final male mould using a tooling gel coat and fibreglass reinforcement

Thanks for the replies everyone!

I should have mentioned that I didn't plan on just laying the carbon fiber over the bondo. I'm still in the planning stages and thought I might put some gelcoat, or another paint like covering on it prior to laying the carbon down. I like the idea of the fiberglass to add some structure to the mold and having resin layer to lay up upon.

I'll keep everyone updated with how everything goes!

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
AlpineCoupe - 6 Years Ago
Hanaldo - 6 Years Ago
AlpineCoupe - 6 Years Ago
SleepingAwake - 6 Years Ago
Mikerw - 6 Years Ago
MarkMK - 6 Years Ago
AlpineCoupe - 6 Years Ago
Hanaldo - 6 Years Ago
             Thank you, that's very helpful!
AlpineCoupe - 6 Years Ago
AlpineCoupe - 6 Years Ago
SleepingAwake - 6 Years Ago
AlpineCoupe - 6 Years Ago
MarkMK - 6 Years Ago
             Thanks! That's a good suggestion!
AlpineCoupe - 6 Years Ago
AlpineCoupe - 6 Years Ago
MarkMK - 6 Years Ago
AlpineCoupe - 6 Years Ago
AlpineCoupe - 5 Years Ago
AlpineCoupe - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search