Hello all, Im new to the forum and new to making composite parts. I have made a couple of splitter vents for a race car of mine and now am working on brake cooling ducts for the front air dam. 

My question is how to lay up the carbon fiber to ensure a reasonable release from the mold. It currently looks like this:




I was thinking I could lay it up (after sanding and smoothing of course), as is, vacuum bag it, and essentially make it as one piece. But as I read a couple of other posts on this forum I started to second guess myself. Any suggestions from the collective?

Thanks in advance!

  
Reply
AlpineCoupe
A
Supreme Being (427 reputation)Supreme Being (427 reputation)Supreme Being (427 reputation)Supreme Being (427 reputation)Supreme Being (427 reputation)Supreme Being (427 reputation)Supreme Being (427 reputation)Supreme Being (427 reputation)Supreme Being (427 reputation)
Group: Forum Members
Posts: 45, Visits: 2.1K
Well got the part made... and ran into a problem when de-molding it.

Turns out the mechanical lock was too much for the connection between the foam and the board I adhered it to. So a one and done mold. On a positive note though, the part looked good when I got all of the foam out of the center!

On to attempt number 2 at making a mold!

Bagged:

Attempted de-molding, and mold failure:


Foam removed, still needs to be trimmed:


GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
AlpineCoupe - 6 Years Ago
Hanaldo - 6 Years Ago
AlpineCoupe - 6 Years Ago
SleepingAwake - 6 Years Ago
Mikerw - 6 Years Ago
MarkMK - 6 Years Ago
AlpineCoupe - 6 Years Ago
Hanaldo - 6 Years Ago
             Thank you, that's very helpful!
AlpineCoupe - 6 Years Ago
AlpineCoupe - 6 Years Ago
SleepingAwake - 6 Years Ago
AlpineCoupe - 6 Years Ago
MarkMK - 6 Years Ago
             Thanks! That's a good suggestion!
AlpineCoupe - 6 Years Ago
AlpineCoupe - 6 Years Ago
MarkMK - 6 Years Ago
AlpineCoupe - 6 Years Ago
AlpineCoupe - 5 Years Ago
AlpineCoupe - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search