I've been looking around for a CNC cutter/laser to cut out certain standard shapes. We mainly use xpreg XC 110 and XC 130 (unidirectional). I came across the CNC-step machines. On their site it says they can cut prepreg with an oscillating knive, but in reality it turns out there are some issues. Does anyone know of a system or manufacturer that allows CNC cutting of prepreg materials?

Rogier
Edited 6 Years Ago by Rogier Claes
Replies
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
I feel nobody is reading what the OP is actually asking haha.

OP, for what it's worth - I have tried an oscillating knife on a 6040 CNC router to cut uncured XC110. It was a disaster. The material tends to grab at the cutter after a few cuts, meaning it will start off cutting ok and then it will randomly grab the cutter and bunch and the cutter will proceed to ruin everything in true CNC fashion. I have no idea if this was due to the quality of the cutter, though it wasn't cheap (cost me about AU$300 for the single blade and holder). I also don't know if I could have got it to work with some effort, I gave up on the idea and decided that any pre-preg I am cutting on a 6040 bed is quick enough to cut by hand, even if it's a bit laborious. 
Steve Broad
Steve Broad
Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
Hanaldo - 12/4/2019 2:11:40 AM
I feel nobody is reading what the OP is actually asking haha.

OP, for what it's worth - I have tried an oscillating knife on a 6040 CNC router to cut uncured XC110. It was a disaster. The material tends to grab at the cutter after a few cuts, meaning it will start off cutting ok and then it will randomly grab the cutter and bunch and the cutter will proceed to ruin everything in true CNC fashion. I have no idea if this was due to the quality of the cutter, though it wasn't cheap (cost me about AU$300 for the single blade and holder). I also don't know if I could have got it to work with some effort, I gave up on the idea and decided that any pre-preg I am cutting on a 6040 bed is quick enough to cut by hand, even if it's a bit laborious. 

Yeah, good point :-)

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Rogier Claes - 6 Years Ago
Warren (Staff) - 6 Years Ago
Rogier Claes - 6 Years Ago
Steve Broad - 6 Years Ago
Fasta - 6 Years Ago
Rogier Claes - 6 Years Ago
Fasta - 6 Years Ago
mahmut - 6 Years Ago
mahmut - 6 Years Ago
Hanaldo - 6 Years Ago
             Yeah, good point :-)
Steve Broad - 6 Years Ago
Kairu - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search