Complex parts perfectly finished on both sides


Author
Message
kerolous Amin
kerolous Amin
Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)
Group: Forum Members
Posts: 2, Visits: 7
How to get a perfect shiny surface on both sides of complex parts?
Method: vacuum infusion
Materials: carbon fiber, epoxy
Reply
kerolous Amin
kerolous Amin
Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)
Group: Forum Members
Posts: 2, Visits: 7
scottracing - 2/1/2019 12:41:59 PM
I'm not great with infusion techniques as i use prepreg mainly, and that's the process I use to make matched tooling and parts that have a good surface finish on both sides.

Can you elaborate on what you are making? and why you have a requirement for both surfaces to be a gloss finish?


something like this tub or the plate both were perfectly surface finished on both sides, I am wondering if it can be accomplished by vacuum infusion and how?
In this video, a very thin release-film has been used for cosmetic appearance  https://www.youtube.com/watch?v=Xm2Ezo70vFI
would it help in making large parts? or it would result in increased weight because of lacking peel-ply.


 













Edited 6 Years Ago by kerolous Amin
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search