By kerolous Amin - 2/1/2019 12:31:21 AM

How to get a perfect shiny surface on both sides of complex parts?
Method: vacuum infusion
Materials: carbon fiber, epoxy
By matthieutje65 - 2/6/2019 7:16:42 PM

the parts you are referring to are made by two seperate infusions on two seperate mould, with gloss finish on outside visible side, then bonded together