Hi guys,

I plan to do a resin infusion as follows: (top to bottom)

bagging film (from starter pack)
160g twill weave
390g twill weave
closed cell foam
390g twill weave
160g twill weave
flat acrylic mould (perspex)

As this is first time I'm going to do this I'm worried if the finished product will be shiny, smooth and glossy on both sides? Or I am missing something here?

Thank you
Replies
pk_090
pk_090
Supreme Being (383 reputation)Supreme Being (383 reputation)Supreme Being (383 reputation)Supreme Being (383 reputation)Supreme Being (383 reputation)Supreme Being (383 reputation)Supreme Being (383 reputation)Supreme Being (383 reputation)Supreme Being (383 reputation)
Group: Forum Members
Posts: 47, Visits: 169
Glass sheet, needs to be a good quality toughened glass, and not laminated. Ideally automotive glass would be good, but finding a flan non curved piece is the tricky part.
Alex
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Mirrors work out great too check this video I've made me making some testsamples.



its not my best video but proves that you can do an infusion on a mirror with a very good finnish!

PS: Before I started using infusion and all that complex stuff, ive made some realy good loocking small, flat parts using wet lamination with plenty of resin and then sandwishing the laminate in between two pieces of laminated wood (I don't know the name in english but it's mdf-wood with a shiny thin (coloured) topcoat.) First I've first only used clamps than improved to vacuumbag the "sandwich" wood - laminate - wood. excess resin was squeezed out. This means you get a good loocking part, but it's more for cosmetic purpose.

Hope this might help you

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




mannime
mannime
Forum Guru (57 reputation)Forum Guru (57 reputation)Forum Guru (57 reputation)Forum Guru (57 reputation)Forum Guru (57 reputation)Forum Guru (57 reputation)Forum Guru (57 reputation)Forum Guru (57 reputation)Forum Guru (57 reputation)
Group: Forum Members
Posts: 7, Visits: 31
Hi Matthieu,

thanks for sharing that video. I'm really interested in your test results. Do you mind sharing them?

Thanks
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Well I did this for personal use, to add to my "material library" I haven't tested them in a lab or something like that so I don't have numbers about their stiffness and strenght.
What I can say is that the PVC foam cored sample is quit strong in ratio to his weight.
A second remarkable thing was the carbonfiber sandwich with fiberglass. I've did Carbon-glas-Carbon-glas-Carbon resulting in a very stiff, but heavier part. 
samples with the carbon only start to get stiff after 5+ layers. When there are less layers its quit easy to bend.

I'll try to upload a new video talking about the weight and more details on the samples in the near future Smile 

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
mannime - 13 Years Ago
r0bsk1 - 13 Years Ago
mannime - 13 Years Ago
r0bsk1 - 13 Years Ago
mannime - 13 Years Ago
r0bsk1 - 13 Years Ago
matthieutje65 - 13 Years Ago
                                 Hi Matthieu, now I'm worried about my plexiglass surface. Any suggestions as to what else I could...
mannime - 13 Years Ago
pk_090 - 13 Years Ago
matthieutje65 - 13 Years Ago
mannime - 13 Years Ago
matthieutje65 - 13 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search