111mattin111
111mattin111
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 67,
Visits: 910
OK need a little help I've done a quick video as well to show what im on about
I've vaccum bagged my lay up and got absolute vaccum, but when I do a drop test leaving it 15min when I come back to it turn the pump on and release the clamp it starts pulling vaccum again then after a few minutes it pulls absolute vaccum again without touching anything,
Is this normal or is something causing it to do this? I don't want to infuse it if airs getting into the bag
Thanks Paul
Reply
Like
3
Reply
111mattin111
111mattin111
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 67,
Visits: 910
I used the hose that comes with the infusion starter kit, which other hose would you recommend?
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Help
111mattin111
-
10 Years Ago
http://s200.photobucket.com/user/rb200/library/?view=recent&page=1
111mattin111
-
10 Years Ago
Well been over the bag a million times and can't find the leak, I can get it to pull vaccum but once...
111mattin111
-
10 Years Ago
Hi Good housekeeping helps regarding leaking bags so make sure you bagging material is stored in a...
carbonfibreworks
-
10 Years Ago
The vac bag has been stored it a sealed bag out of the way, Would it still be able to pull full vac...
111mattin111
-
10 Years Ago
Hi One way to check it is envelope bag the mould but make sure the back of the mould has been sanded...
carbonfibreworks
-
10 Years Ago
Not sure I'd be able to envelope bag it due to the size and weight of the mould, Hmmmm not really...
111mattin111
-
10 Years Ago
Hi Just try re bagging first. Regards Chris
carbonfibreworks
-
10 Years Ago
Ive found most leaks are around the tape and especially at the vacuum intake and outlet at the bag...
VVS
-
10 Years Ago
to answer your question if you do not have a digital vacuumreader you can get "full" vacuum on the...
matthieutje65
-
10 Years Ago
Ok so sorted the leak out and no pressure drop after couple of hours then the nightmare started...
111mattin111
-
10 Years Ago
Just ironing out the kinks mate, happens to everyone when they first start infusing. Keep at it,...
Hanaldo
-
10 Years Ago
I used the hose that comes with the infusion starter kit, which other hose would you recommend?
111mattin111
-
10 Years Ago
I see. Well in that case, I'd probably get in contact with the guys at EC, as their stuff definitely...
Hanaldo
-
10 Years Ago
I thought that, I now think it was definitely down to collapsed pipes as soon as I changed them it...
111mattin111
-
10 Years Ago
I have used the EC clear hose many times and the only time it has collapsed is when its been too...
carbonfibreworks
-
10 Years Ago
I mixed the resin with slow hardner, I didn't have any blow heaters on it was done in the house, the...
111mattin111
-
10 Years Ago
OK so that's a slightly different issue and can happen with this type of hose, when you have started...
carbonfibreworks
-
10 Years Ago
I did try that putting the clamp back on and trying to squash the pipe back the other way, I think...
111mattin111
-
10 Years Ago
Was your resin feed pot positioned below the part? If it was higher the liquid resin could siphon...
Frobisher
-
10 Years Ago
Yes the pot was slightly higher than part so would explain the puddle of resin, does everyone else...
111mattin111
-
10 Years Ago
I've had a few instances of the clear EC pipe squashing flat under vacuum .. :( It usually happens...
Dravis
-
10 Years Ago
Great tip thanks for that I'll try this next time
111mattin111
-
10 Years Ago
Paul, Can you highlight where you store your resin and hardner and at what temperature they are...
Superleggera
-
10 Years Ago
There stored in my workshop which does get cold at night is this no good? Before I mixed they were...
111mattin111
-
10 Years Ago
Paul, I keep my IN2 and AT30 stored at about 25 degrees and it lowers the viscosity significantly....
Superleggera
-
10 Years Ago
Just to add to the previous points - I've found that, nearly all the time, leaks haveactually...
MarkMK
-
10 Years Ago
As far as I've read this topic, one question hasn't been asked...Do you infuse on top of the...
matthieutje65
-
10 Years Ago
[quote][b]111mattin111 (01/11/2015)[/b][hr] OK need a little help I've done a quick video as well...
fgayford
-
10 Years Ago
Thanks for the advice and replies not had chance to do my second lay up yet but will be doing one...
111mattin111
-
10 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search