Group: Forum Members
Posts: 346,
Visits: 4.4K
|
Unless you're making top end components, you don't need an autoclave, ooac pre preg covers most aspects now, and given the cost of maintaining and buying an autoclave, most people can live with the little bit of extra weight from a couple extra layers
|