Where can O find the spray that stick the fabric to the mould ?
Where can O find the spray that stick the fabric to the mould ?
Post Reply
Like
3
Where can O find the spray that stick the fabric to the mould ?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Jess8bit
Jess8bit
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 133,
Visits: 566
In video tutorial
How to Make a Carbon Fibre Car Bonnet/Hood - Part 2/3
at about 03'22' you are using a spray that helps you to maintain the fabric.
What is it and where can I find it in the webstore ?
thank you
Reply
Like
3
Reply
mikew
mikew
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 56,
Visits: 128
Guys, I'm still using this Elmers stuff, made many parts with it including very tricky shapes with tight corners - no issues whatsoever and its incredibly cheap.
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Where can O find the spray that stick the fabric to the mould ?
Jess8bit
-
13 Years Ago
Apparently there is a problem with the manufacturer, it has been showing "out of stock" on the EC...
wozza
-
13 Years Ago
[quote][b]wozza (17/11/2012)[/b][hr]Apparently there is a problem with the manufacturer, it has been...
Jess8bit
-
13 Years Ago
I bought a product called elmers repositionable spray, it's clear pva light adhesive. If you lightly...
mikew
-
13 Years Ago
[quote][b]mikew (18/11/2012)[/b][hr]I bought a product called elmers repositionable spray, it's...
Jess8bit
-
13 Years Ago
Some people use 3M spray. I talked to a large manufacturer at at a trade show. I asked what they...
fgayford
-
13 Years Ago
[quote][b]fgayford (18/11/2012)[/b][hr]Some people use 3M spray. I talked to a large manufacturer at...
Jess8bit
-
13 Years Ago
Nice to hear of that theory of hairspray. In addition on that I can say; not to use "normal hobby...
matthieutje65
-
13 Years Ago
The one thing I have learned in composites is this. Listen and if it makes sense test it yourself....
fgayford
-
13 Years Ago
All my entire project I used scotch spray mount and there is no problem in CF part quality...
Leon
-
13 Years Ago
thank guys, seems like 3M spray is a good candidate.
Jess8bit
-
13 Years Ago
I have used 3M 77 (which is the industrial strength stuff) I think it is too much. It sticks very...
baja_patient
-
13 Years Ago
[quote][b]baja_patient (19/11/2012)[/b][hr]I have used 3M 77 (which is the industrial strength...
star.ace
-
12 Years Ago
Yeah star.ace, it seems Zyvax have serious production issue, from what I've heard recently.
Jess8bit
-
12 Years Ago
Thanks a lot for your feedback ! :)
Jess8bit
-
13 Years Ago
I've heard the hairspray idea before, never tried it myself but tempted to soon
ajb100
-
13 Years Ago
[quote][b]ajb100 (19/11/2012)[/b][hr]I've heard the hairspray idea before, never tried it myself but...
Jess8bit
-
13 Years Ago
I use Stayz from Zyvax as it is epoxy compatiable. Should be available from Composites One and...
w10n320wt
-
12 Years Ago
[quote][b]w10n320wt (04/04/2013)[/b][hr]I use Stayz from Zyvax as it is epoxy compatiable. Should be...
Jess8bit
-
12 Years Ago
[quote][b]Jess8bit (04/04/2013)[/b][hr][quote][b]w10n320wt (04/04/2013)[/b][hr]I use Stayz from...
GROPIUS
-
12 Years Ago
thank you Gropius :w00t:
Jess8bit
-
12 Years Ago
What a reseller in Italy told me is that stayz was going to cure in the cans in two weeks time. So...
alebassa
-
12 Years Ago
[quote][b]alebassa (04/04/2013)[/b][hr]What a reseller in Italy told me is that stayz was going to...
Jess8bit
-
12 Years Ago
This is the stuff I've been using...
ajb100
-
12 Years Ago
[quote][b]ajb100 (05/04/2013)[/b][hr]This is the stuff I've been using...
Jess8bit
-
12 Years Ago
Could we get some info from EasyComposites to regarding the in-can shelf life of StayZ? I have used...
baja_patient
-
12 Years Ago
Why the hell did I miss that 3M product !? :blush: Sounds perfect ! Where can we find it in...
Jess8bit
-
12 Years Ago
Hi I have a good story about the spray adhesive, seeking Stayz discovered that the distributor for...
Manu
-
12 Years Ago
OK. :) By the way, I live in Europe (near Paris) and this week I've tried to be delivered a box...
Jess8bit
-
12 Years Ago
I have tried "Infutac" from french Diatex, holds thing in place nicely but leaves fiber trace on the...
prsw
-
12 Years Ago
Guys, I'm still using this Elmers stuff, made many parts with it including very tricky shapes with...
mikew
-
12 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search