Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Resin Infusion
»
Where can O find the spray that stick the fabric to the mould ?
Where can O find the spray that stick the fabric to the mould ?
Post Reply
Like
3
Where can O find the spray that stick the fabric to the mould ?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Jess8bit
Jess8bit
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 133,
Visits: 566
In video tutorial
How to Make a Carbon Fibre Car Bonnet/Hood - Part 2/3
at about 03'22' you are using a spray that helps you to maintain the fabric.
What is it and where can I find it in the webstore ?
thank you
Reply
Like
3
Replies
Manu
Manu
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 23,
Visits: 435
Hi I have a good story about the spray adhesive, seeking Stayz discovered that the distributor for Europe was less than 70km from my city, I contacted them and they said they had saved hundreds of spray they could not sell because they were defective, that if I wanted to try them gave me one. When I visit his shop to catch the spray. Indeed its spray is defective, to used once, the next day it was all stuck and useless. From then probe different products and brands, it is certainly my choice spraymount 3m, and I have made many infusions and the result is perfect, even among gc50 gelcoat and the first layer of carbon fiber.
www.ktuning.es  
https://www.facebook.com/Ktuning.es/ 
www.carboncycleparts.com 
https://www.facebook.com/CarbonCycleParts/
Attachments
P4060087.jpg
(
382 views,
4.00 KB
)
P4060089.jpg
(
383 views,
18.00 KB
)
Edited
12 Years Ago by
Manu
Reply
Like
3
Jess8bit
Jess8bit
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 133,
Visits: 566
OK.
By the way, I live in Europe (near Paris) and this week I've tried to be delivered a box of 3M ACPS from US retailers, but it is impossible. They are not allowed to ship it this way
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Where can O find the spray that stick the fabric to the mould ?
Jess8bit
-
13 Years Ago
Apparently there is a problem with the manufacturer, it has been showing "out of stock" on the EC...
wozza
-
13 Years Ago
[quote][b]wozza (17/11/2012)[/b][hr]Apparently there is a problem with the manufacturer, it has been...
Jess8bit
-
13 Years Ago
I bought a product called elmers repositionable spray, it's clear pva light adhesive. If you lightly...
mikew
-
13 Years Ago
[quote][b]mikew (18/11/2012)[/b][hr]I bought a product called elmers repositionable spray, it's...
Jess8bit
-
13 Years Ago
Some people use 3M spray. I talked to a large manufacturer at at a trade show. I asked what they...
fgayford
-
13 Years Ago
[quote][b]fgayford (18/11/2012)[/b][hr]Some people use 3M spray. I talked to a large manufacturer at...
Jess8bit
-
13 Years Ago
Nice to hear of that theory of hairspray. In addition on that I can say; not to use "normal hobby...
matthieutje65
-
13 Years Ago
The one thing I have learned in composites is this. Listen and if it makes sense test it yourself....
fgayford
-
13 Years Ago
All my entire project I used scotch spray mount and there is no problem in CF part quality...
Leon
-
13 Years Ago
thank guys, seems like 3M spray is a good candidate.
Jess8bit
-
13 Years Ago
I have used 3M 77 (which is the industrial strength stuff) I think it is too much. It sticks very...
baja_patient
-
13 Years Ago
[quote][b]baja_patient (19/11/2012)[/b][hr]I have used 3M 77 (which is the industrial strength...
star.ace
-
12 Years Ago
Yeah star.ace, it seems Zyvax have serious production issue, from what I've heard recently.
Jess8bit
-
12 Years Ago
Thanks a lot for your feedback ! :)
Jess8bit
-
13 Years Ago
I've heard the hairspray idea before, never tried it myself but tempted to soon
ajb100
-
13 Years Ago
[quote][b]ajb100 (19/11/2012)[/b][hr]I've heard the hairspray idea before, never tried it myself but...
Jess8bit
-
13 Years Ago
I use Stayz from Zyvax as it is epoxy compatiable. Should be available from Composites One and...
w10n320wt
-
12 Years Ago
[quote][b]w10n320wt (04/04/2013)[/b][hr]I use Stayz from Zyvax as it is epoxy compatiable. Should be...
Jess8bit
-
12 Years Ago
[quote][b]Jess8bit (04/04/2013)[/b][hr][quote][b]w10n320wt (04/04/2013)[/b][hr]I use Stayz from...
GROPIUS
-
12 Years Ago
thank you Gropius :w00t:
Jess8bit
-
12 Years Ago
What a reseller in Italy told me is that stayz was going to cure in the cans in two weeks time. So...
alebassa
-
12 Years Ago
[quote][b]alebassa (04/04/2013)[/b][hr]What a reseller in Italy told me is that stayz was going to...
Jess8bit
-
12 Years Ago
This is the stuff I've been using...
ajb100
-
12 Years Ago
[quote][b]ajb100 (05/04/2013)[/b][hr]This is the stuff I've been using...
Jess8bit
-
12 Years Ago
Could we get some info from EasyComposites to regarding the in-can shelf life of StayZ? I have used...
baja_patient
-
12 Years Ago
Why the hell did I miss that 3M product !? :blush: Sounds perfect ! Where can we find it in...
Jess8bit
-
12 Years Ago
Hi I have a good story about the spray adhesive, seeking Stayz discovered that the distributor for...
Manu
-
12 Years Ago
OK. :) By the way, I live in Europe (near Paris) and this week I've tried to be delivered a box...
Jess8bit
-
12 Years Ago
I have tried "Infutac" from french Diatex, holds thing in place nicely but leaves fiber trace on the...
prsw
-
12 Years Ago
Guys, I'm still using this Elmers stuff, made many parts with it including very tricky shapes with...
mikew
-
12 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search