I have been working on an aircraft repair. The plane is constructed out of some kind of a core that I have never seen before.

The best description I can give is that it looks like cardboard looking through it from a cut panel edge of it. It has 2 skins one outer and one inner with long open cells going through the length of it exactly like a cardboard box material looks. Another description would be that it looks like coroplast sign board.

I believe it is vinylester and glass. Any help would be much appreciated.

Thanks

Fred 
Reply
fgayford
fgayford
Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
carboncactus (09/06/2013)
Alumalite?

Whatever it is, it sounds like a unidirectional corrugated core.
 
 Thanks, I took a look at Alumalite and it looks the same only my sample is definitely glass fibre resin formed in a concave mold.

Could it be some sort of prepreg sheeting?

Fred 