Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Pre-Pregs
»
Information needed
Information needed
Post Reply
Like
2
Information needed
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
fgayford
fgayford
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 433,
Visits: 1.2K
carboncactus (09/06/2013)
Alumalite?
Whatever it is, it sounds like a unidirectional corrugated core.
Thanks, I took a look at Alumalite and it looks the same only my sample is definitely glass fibre resin formed in a concave mold.
Could it be some sort of prepreg sheeting?
Fred
Reply
Like
2
carboncactus
carboncactus
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 243,
Visits: 1K
Alumalite?
Whatever it is, it sounds like a unidirectional corrugated core.
Edited
12 Years Ago by
carboncactus
Reply
Like
3
fgayford
fgayford
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 433,
Visits: 1.2K
I have been working on an aircraft repair. The plane is constructed out of some kind of a core that I have never seen before.
The best description I can give is that it looks like cardboard looking through it from a cut panel edge of it. It has 2 skins one outer and one inner with long open cells going through the length of it exactly like a cardboard box material looks. Another description would be that it looks like coroplast sign board.
I believe it is vinylester and glass. Any help would be much appreciated.
Thanks
Fred
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search