Group: Forum Members
Posts: 433,
Visits: 1.2K
|
I have been working on an aircraft repair. The plane is constructed out of some kind of a core that I have never seen before.
The best description I can give is that it looks like cardboard looking through it from a cut panel edge of it. It has 2 skins one outer and one inner with long open cells going through the length of it exactly like a cardboard box material looks. Another description would be that it looks like coroplast sign board.
I believe it is vinylester and glass. Any help would be much appreciated.
Thanks
Fred
|