I am going to vacuum bag a Carbon Fiber bar stool, using IN2 Resin, Soric and Carbon Fiber Tape at the edges of the Soric, like in the How To...Bonnet/Hood video. The stool will be like a 16-inch wide ribbon with a profile that looks like a "Z", and a Soric core. The total length is approximately 65-inches. I am in the US, and I cannot find Infusion Grade Spray Tack anywhere.

What method/s (other than Spray Tack) could I use to hold the Carbon Fiber Tape, Cloth, and Soric in place?

Many Thanks!
Reply
Fredrik Welen
Fredrik Welen
Supreme Being (767 reputation)Supreme Being (767 reputation)Supreme Being (767 reputation)Supreme Being (767 reputation)Supreme Being (767 reputation)Supreme Being (767 reputation)Supreme Being (767 reputation)Supreme Being (767 reputation)Supreme Being (767 reputation)
Group: Forum Members
Posts: 53, Visits: 478
I don´t know why i didn´t think of that. Thanks for reminding me.  I will add easy lease again and try again.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
ModShane - 12 Years Ago
Warren (Staff) - 12 Years Ago
matthieutje65 - 12 Years Ago
Dan22h - 9 Years Ago
Matt (Staff) - 9 Years Ago
Dan22h - 9 Years Ago
Fredrik Welen - 4 Years Ago
                 try spraying the spray tack onto the fabric.
SleepingAwake - 4 Years Ago
Hanaldo - 12 Years Ago
Dravis - 12 Years Ago
brainfart - 12 Years Ago
Dravis - 12 Years Ago
brainfart - 12 Years Ago
Billis21 - 9 Years Ago
Billis21 - 9 Years Ago
Matt (Staff) - 9 Years Ago
Warren (Staff) - 9 Years Ago
Dan22h - 9 Years Ago
Dezer - 9 Years Ago
Dan22h - 9 Years Ago
fgayford - 9 Years Ago
Warren (Staff) - 9 Years Ago
Billis21 - 9 Years Ago
DANNYHOCKIN - 9 Years Ago
Fredrik Welen - 4 Years Ago
Hanaldo - 4 Years Ago
             Which spray are you using now Hanaldo?
chriscnf - 4 Years Ago
SleepingAwake - 4 Years Ago