Infusion grade spray tack alternative


Author
Message
ModShane
ModShane
Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)
Group: Forum Members
Posts: 1, Visits: 20
I am going to vacuum bag a Carbon Fiber bar stool, using IN2 Resin, Soric and Carbon Fiber Tape at the edges of the Soric, like in the How To...Bonnet/Hood video. The stool will be like a 16-inch wide ribbon with a profile that looks like a "Z", and a Soric core. The total length is approximately 65-inches. I am in the US, and I cannot find Infusion Grade Spray Tack anywhere.

What method/s (other than Spray Tack) could I use to hold the Carbon Fiber Tape, Cloth, and Soric in place?

Many Thanks!
Reply
Dravis
Dravis
Supreme Being (7.2K reputation)Supreme Being (7.2K reputation)Supreme Being (7.2K reputation)Supreme Being (7.2K reputation)Supreme Being (7.2K reputation)Supreme Being (7.2K reputation)Supreme Being (7.2K reputation)Supreme Being (7.2K reputation)Supreme Being (7.2K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
Cytec Aerofix 3 is available from "www.ecfibreglasssupplies.co.uk" at around £12,-

http://www.ecfibreglasssupplies.co.uk/p-2961-aerofix-3-spray-adhesive.aspx


Unfortunately they will not ship anything to Denmark ... Pinch

I'll have to find a way to get it shipped here ... Doze


The "homemade" spray tack is probably by far the most economical way, and not a problem if you have a production of larger parts running.
You can make up a batch of the spray tack, and use it up, then clean the bottle ...

When you're only making a few smaller parts a month/week, then the spray tack in a can is a lot more convenient...

I've used ordinary 3M spray on the intermediate layers, where it makes no diffference, since the spray tack is not seen, but I am a bit worried if it impairs the final strength of the laminate.

The "homemade spray tack" is a bit inconvenient here, since you need to leave it to cure to a tack...  which means hours between layers, and new batches of spray made up ...
(unless it works if you put the mixture in the freezer ??)




 


"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
Edited 12 Years Ago by Dravis
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
ModShane - 12 Years Ago
Warren (Staff) - 12 Years Ago
matthieutje65 - 12 Years Ago
Dan22h - 9 Years Ago
Matt (Staff) - 9 Years Ago
Dan22h - 9 Years Ago
Fredrik Welen - 4 Years Ago
                 try spraying the spray tack onto the fabric.
SleepingAwake - 4 Years Ago
Hanaldo - 12 Years Ago
Dravis - 12 Years Ago
brainfart - 12 Years Ago
Dravis - 12 Years Ago
brainfart - 12 Years Ago
Billis21 - 9 Years Ago
Billis21 - 9 Years Ago
Matt (Staff) - 9 Years Ago
Warren (Staff) - 9 Years Ago
Dan22h - 9 Years Ago
Dezer - 9 Years Ago
Dan22h - 9 Years Ago
fgayford - 9 Years Ago
Warren (Staff) - 9 Years Ago
Billis21 - 9 Years Ago
DANNYHOCKIN - 9 Years Ago
Fredrik Welen - 4 Years Ago
Hanaldo - 4 Years Ago
             Which spray are you using now Hanaldo?
chriscnf - 4 Years Ago
SleepingAwake - 4 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search