Infusion grade spray tack alternative


Author
Message
ModShane
ModShane
Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)
Group: Forum Members
Posts: 1, Visits: 20
I am going to vacuum bag a Carbon Fiber bar stool, using IN2 Resin, Soric and Carbon Fiber Tape at the edges of the Soric, like in the How To...Bonnet/Hood video. The stool will be like a 16-inch wide ribbon with a profile that looks like a "Z", and a Soric core. The total length is approximately 65-inches. I am in the US, and I cannot find Infusion Grade Spray Tack anywhere.

What method/s (other than Spray Tack) could I use to hold the Carbon Fiber Tape, Cloth, and Soric in place?

Many Thanks!
Replies
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
That definitely sounds like way too much meths in the mix. we would normally be using around 10-15% max which should be enough to spray it through most "spritzer" type bottles. Although its not something we have seen before, it does seem that excessive meths has somehow effected the efficiency of EasyLease in this case.

In our opinion, the best solution for your problem, especially as you are using glass fibre is to use our FusionFix GP Spray Adhesive. As you are using glassfibre rather than cosmetic carbon, any slight issues on the surface will easily polish off and we also know from experience that Fusion Fix does not impact on release agents.



Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Dan22h
Dan22h
Supreme Being (175 reputation)Supreme Being (175 reputation)Supreme Being (175 reputation)Supreme Being (175 reputation)Supreme Being (175 reputation)Supreme Being (175 reputation)Supreme Being (175 reputation)Supreme Being (175 reputation)Supreme Being (175 reputation)
Group: Forum Members
Posts: 15, Visits: 197
Warren (Staff) - 9/14/2017 4:09:29 PM
That definitely sounds like way too much meths in the mix. we would normally be using around 10-15% max which should be enough to spray it through most "spritzer" type bottles. Although its not something we have seen before, it does seem that excessive meths has somehow effected the efficiency of EasyLease in this case.

In our opinion, the best solution for your problem, especially as you are using glass fibre is to use our FusionFix GP Spray Adhesive. As you are using glassfibre rather than cosmetic carbon, any slight issues on the surface will easily polish off and we also know from experience that Fusion Fix does not impact on release agents.


I'm actually making cosmetic carbon, I was using the fibre glass version as a tester to see how it went first before committing to the carbon.The fibreglass version is being used by someone who will be painting it anyway. I'll give it a try with less 10% methylated spirits next time.

Dezer
Dezer
Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)
Group: Forum Members
Posts: 74, Visits: 1.8K
[citar]
[b]Warren (Staff) - 14/09/2017 4:09:29 PM[/ b]
Isso definitivamente parece ser uma forma de metanhas demais na mistura. nós normalmente estaríamos usando cerca de 10-15% no máximo, o que deveria ser suficiente para pulverizá-lo através da maioria dos frascos tipo "spritzer". Embora não seja algo que já vimos antes, parece que as metanfetamensas excessivas têm de alguma forma efetuado a eficiência da EasyLease neste caso.

Na nossa opinião, a melhor solução para o seu problema, especialmente porque você está usando fibra de vidro é usar nosso adesivo de pulverização FusionFix GP. Como você está usando fibra de vidro ao invés de carbono cosmético, quaisquer problemas ligeiros na superfície serão facilmente polidos e também sabemos por experiência que a Fusion Fix não afeta os agentes de liberação.

[/citar]


Can I replace methylated spirit with pure acetone? In my country I have difficulty buying methylated spirit.

Edited 9 Years Ago by Dezer
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
ModShane - 12 Years Ago
Warren (Staff) - 12 Years Ago
matthieutje65 - 12 Years Ago
Dan22h - 9 Years Ago
Matt (Staff) - 9 Years Ago
Dan22h - 9 Years Ago
Fredrik Welen - 4 Years Ago
                 try spraying the spray tack onto the fabric.
SleepingAwake - 4 Years Ago
Hanaldo - 12 Years Ago
Dravis - 12 Years Ago
brainfart - 12 Years Ago
Dravis - 12 Years Ago
brainfart - 12 Years Ago
Billis21 - 9 Years Ago
Billis21 - 9 Years Ago
Matt (Staff) - 9 Years Ago
Warren (Staff) - 9 Years Ago
Dan22h - 9 Years Ago
Dezer - 9 Years Ago
Dan22h - 9 Years Ago
fgayford - 9 Years Ago
Warren (Staff) - 9 Years Ago
Billis21 - 9 Years Ago
DANNYHOCKIN - 9 Years Ago
Fredrik Welen - 4 Years Ago
Hanaldo - 4 Years Ago
             Which spray are you using now Hanaldo?
chriscnf - 4 Years Ago
SleepingAwake - 4 Years Ago