This is probably a silly question, but to use the unimould system on a epoxy coating resin finished plug, do I need to use a release agent before putting down the first tooling coat?

Thanks,
James
Reply
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi James,

Not much to add really, I'd offer the same advice as Warren. You would need release agent on the epoxy coating resin covered pattern; several coats on a new mould, just as he's said. It will be a pretty reliable release though (polyester and vinylester really don't like sticking to epoxy).

All the best, Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search