Hi Dennis,
Mmmm, yes, the sequence if you use Easy-Lease and wax together is very importantly Easy-Lease first, wax second. If you do it the other way round the Easy-Lease will effectively remove the wax but at the same time contaminate the Easy-Lease so you've got neather a was or a chemical release agent barrier. In the correct order there is no reason why the release shouldn't be perfect, leaving both the pattern and the mould as they were.
--Matt
Matt Statham Easy Composites / Carbon Mods - Technical Sales
|