Do I need a release agent?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
jamesw
jamesw
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 61,
Visits: 558
This is probably a silly question, but to use the unimould system on a epoxy coating resin finished plug, do I need to use a release agent before putting down the first tooling coat?
Thanks,
James
Reply
Like
4
Reply
jamesw
jamesw
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 61,
Visits: 558
Would you recommend I be using PVA or easy-lease? (this is the first time the pattern will be used)
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Do I need a release agent?
jamesw
-
13 Years Ago
Yes. and on a new mould/plug use plenty.
wozza
-
13 Years Ago
Would you recommend I be using PVA or easy-lease? (this is the first time the pattern will be used)
jamesw
-
13 Years Ago
I am an Easy Lease convert ha ha. It is brilliant stuff, that's all I use these days. It is quick...
wozza
-
13 Years Ago
Hi James, Not much to add really, I'd offer the same advice as Warren. You would need release agent...
Matt (Staff)
-
13 Years Ago
Many thanks, will get an order in today! James
jamesw
-
13 Years Ago
I am getting ready to make some molds.....I have the plugs all done except for wwet sanding and...
Dennis G
-
13 Years Ago
Hi Dennis, It really depends on what your plug is made from and what you have used as the...
wozza
-
13 Years Ago
The finish is 2k primer over body filler. So it "should" have a good bond. I did find out what...
Dennis G
-
13 Years Ago
Hi Dennis, Mmmm, yes, the sequence if you use Easy-Lease and wax together is very importantly...
Matt (Staff)
-
13 Years Ago
Post Reply
Like
4
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search