By jamesw - 12/12/2012 7:03:00 PM
This is probably a silly question, but to use the unimould system on a epoxy coating resin finished plug, do I need to use a release agent before putting down the first tooling coat?
Thanks, James
|
By Matt (Staff) - 12/17/2012 8:41:14 AM
Hi Dennis,
Mmmm, yes, the sequence if you use Easy-Lease and wax together is very importantly Easy-Lease first, wax second. If you do it the other way round the Easy-Lease will effectively remove the wax but at the same time contaminate the Easy-Lease so you've got neather a was or a chemical release agent barrier. In the correct order there is no reason why the release shouldn't be perfect, leaving both the pattern and the mould as they were.
--Matt
|
|