applying release agent on anodized surface


Author
Message
hadi1990
h
Supreme Being (207 reputation)Supreme Being (207 reputation)Supreme Being (207 reputation)Supreme Being (207 reputation)Supreme Being (207 reputation)Supreme Being (207 reputation)Supreme Being (207 reputation)Supreme Being (207 reputation)Supreme Being (207 reputation)
Group: Forum Members
Posts: 15, Visits: 651
Hello,

I want to use aluminium tube as a mandrel for making carbon fibre tubes (using prepreg). but the tube surface is Anodized.
can i apply release agent on a anodized surface?

Thx
Replies
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Nah I don't mean a tool sealer, I mean as part of the anodizing process the anodizing should be sealed afterwards. Not all places will do it without it being requested, because there can also be benefits to unsealed - one of them being an unsealed anodized surface is very easy to bond to. 

A sealed anodized mandrel should not present any issues for release.
Lester Populaire
L
Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
Hanaldo - 5/27/2020 10:53:06 AM
Nah I don't mean a tool sealer, I mean as part of the anodizing process the anodizing should be sealed afterwards. Not all places will do it without it being requested, because there can also be benefits to unsealed - one of them being an unsealed anodized surface is very easy to bond to. 

A sealed anodized mandrel should not present any issues for release.

Ah sorry now i understand. It was a commercially available tube i would assume it was sealed. But as i mentioned before I only ever tried this one part so who knows what happened...