applying release agent on anodized surface


Author
Message
hadi1990
h
Supreme Being (277 reputation)Supreme Being (277 reputation)Supreme Being (277 reputation)Supreme Being (277 reputation)Supreme Being (277 reputation)Supreme Being (277 reputation)Supreme Being (277 reputation)Supreme Being (277 reputation)Supreme Being (277 reputation)
Group: Forum Members
Posts: 15, Visits: 651
Hello,

I want to use aluminium tube as a mandrel for making carbon fibre tubes (using prepreg). but the tube surface is Anodized.
can i apply release agent on a anodized surface?

Thx
Replies
Lester Populaire
L
Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
@ Hanaldo
Did you make tubing with an anodized mandrel? I had some major release problems when i tested that as the tube was mechanically locked on the mandrel after curing as the anodized surface is quite textured.
It was on small diameter tubes tho.
Hanaldo
Hanaldo
Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Lester Populaire - 5/26/2020 6:16:04 PM
@ Hanaldo
Did you make tubing with an anodized mandrel? I had some major release problems when i tested that as the tube was mechanically locked on the mandrel after curing as the anodized surface is quite textured.
It was on small diameter tubes tho.

Was your mandrel sealed? Anodizing itself is quite porous, and needs to be sealed afterwards. Once sealed, it should not have any surface texture or porosity that will cause a mechanical lock.

Lester Populaire
L
Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
Hanaldo - 5/27/2020 12:11:37 AM
Lester Populaire - 5/26/2020 6:16:04 PM
@ Hanaldo
Did you make tubing with an anodized mandrel? I had some major release problems when i tested that as the tube was mechanically locked on the mandrel after curing as the anodized surface is quite textured.
It was on small diameter tubes tho.

Was your mandrel sealed? Anodizing itself is quite porous, and needs to be sealed afterwards. Once sealed, it should not have any surface texture or porosity that will cause a mechanical lock.

No i didn't use any tool sealer, however i used a wax based release agent that is usually pretty good at filling little pits. And i know the release was good as it came off once i cut the tube open.