+x Lester Populaire - 5/26/2020 6:16:04 PM@ HanaldoDid you make tubing with an anodized mandrel? I had some major release problems when i tested that as the tube was mechanically locked on the mandrel after curing as the anodized surface is quite textured.It was on small diameter tubes tho.
+x Hanaldo - 5/27/2020 12:11:37 AM+x Lester Populaire - 5/26/2020 6:16:04 PM@ HanaldoDid you make tubing with an anodized mandrel? I had some major release problems when i tested that as the tube was mechanically locked on the mandrel after curing as the anodized surface is quite textured.It was on small diameter tubes tho.Was your mandrel sealed? Anodizing itself is quite porous, and needs to be sealed afterwards. Once sealed, it should not have any surface texture or porosity that will cause a mechanical lock.