Daz
Daz
posted 14 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 93,
Visits: 651
I have just got this off my shelf in the workshop to use,
I recently bought some new ,
now putting the bottles together the older one on the right looks a totally different colour to the new one,
Both of the bottles are unopened,
I keep them up on a shelf in the dark ,
What i want to know Is it still ok to use or not ??
Dont want to waste a lot of carbon and kevlar,
Any views on this ,
Thanks in advance.
Edited
14 Years Ago by
Daz
Reply
Like
6
Reply
Daz
Daz
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 93,
Visits: 651
Cheers Matt,
Have used it on a battery box lid and it has cured,
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
ET 30 FAST HARDENER PROBLEM ????
Daz
-
14 Years Ago
I guess the guys of Easycomposites can give you more information on that , but what you could do is...
matthieutje65
-
14 Years Ago
Hi Daz, You'll be fine. From the time the hardeners are manufactured, the material starts changing...
Matt (Staff)
-
14 Years Ago
Cheers Matt, Have used it on a battery box lid and it has cured,
Daz
-
14 Years Ago
Post Reply
Like
6
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search