I have just got this off my shelf in the workshop to use,

I recently bought some new ,

now putting the bottles together the older one on the right looks a totally different colour to the new one,

Both of the bottles are unopened,

I keep them up on a shelf in the dark ,

What i want to know Is it still ok to use or not ??

Dont want to waste a lot of carbon and kevlar,

Any views on this ,

Thanks in advance.


Edited 14 Years Ago by Daz
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search