Talk Composites - The Forum for Advanced Composites

ET 30 FAST HARDENER PROBLEM ????

http://www.talkcomposites.com/Topic3550.aspx

By Daz - 11/25/2012 7:13:47 PM

I have just got this off my shelf in the workshop to use,

I recently bought some new ,

now putting the bottles together the older one on the right looks a totally different colour to the new one,

Both of the bottles are unopened,

I keep them up on a shelf in the dark ,

What i want to know Is it still ok to use or not ??

Dont want to waste a lot of carbon and kevlar,

Any views on this ,

Thanks in advance.

By Daz - 11/26/2012 6:05:20 PM

Cheers Matt,

Have used it on a battery box lid and it has cured,