Group: Forum Members
Posts: 680,
Visits: 1.9K
|
Hi Daz,
You'll be fine. From the time the hardeners are manufactured, the material starts changing colour. It's not a function of UV exposure (which is why your hardeners have noth been stored in the dark but are now different colours), instead it will be the case that these two have been poured from two different barrels and would have been manufactured at slightly different times.
I'm totally confident that if we've supplied these in the last 12 months they will be perfectly fine to use and will both cure properly and fully.
All the best, Matt
Matt Statham Easy Composites / Carbon Mods - Technical Sales
|