BoB_from_jungle
BoB_from_jungle
posted 5 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 7,
Visits: 54
Hi guys!
I'm beginner laminator so I will be appretiate you for you help.
I have a round shaped mold. There is common 2 plies of 200 g 4H satin carbon fabric and extra 4 plies on the other area (support area).
I have no idea how to impregnate this one by minimal quantity of resin. I guess I need at least two points of resin feed. One of this needed to be in the geometrical center of support area.
Thanks
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Infusion strategy
BoB_from_jungle
-
5 Years Ago
Hi Bob, the situation isn't clear to me, I can't understand the shape of your mold and where you must put carbon and resin. Can you elaborate it a little better? Maybe some picture of the mold.
Buchado
-
5 Years Ago
Hi In fact my part is oval shaped as I've drawn above (not round shaped) It's a flat part as well but has two plies on the whole area of the part and extra four plies on the area that I've drawn...
BoB_from_jungle
-
5 Years Ago
I may not be understanding right but my suggestions would be to place the feed line over (or along the edge if you're worried about printing - or pull the spiral wrap up in a pleat before it gels) th...
explorecomposites
-
5 Years Ago
Looks like very simple shape and laminate. Is this a cosmetic type part that really needs infusion for a great finish? You could also consider just a wet layup with vacuum bagging using perf film.....
Fasta
-
5 Years Ago
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search