By BoB_from_jungle - 3/1/2020 12:12:10 PM
Hi guys! I'm beginner laminator so I will be appretiate you for you help.
 I have a round shaped mold. There is common 2 plies of 200 g 4H satin carbon fabric and extra 4 plies on the other area (support area). I have no idea how to impregnate this one by minimal quantity of resin. I guess I need at least two points of resin feed. One of this needed to be in the geometrical center of support area. Thanks
|
By Fasta - 3/26/2020 7:18:38 AM
Looks like very simple shape and laminate.
Is this a cosmetic type part that really needs infusion for a great finish?
You could also consider just a wet layup with vacuum bagging using perf film and breather etc as this will be much easier for a beginner than the infusion, would still have good resin ration but may not be the 100% cosmetic finish you want?
|
|