Unfortunately no off the shelf solvents will touch cured adhesive. Also The bond strength is typically higher than the interlaminar sheer strength of carbon fibre so ripping it apart is likely to lead to the carbon delaminating before the glue goes. If you have a reasonable bond gap, abrading away the adhesive is likely the best way.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|