Hi,
I want to seperate a fillament wound carbon tube from a steel bicycle frame that was bonded using Vuduglu 
Can this be done without cutting the tube or damaging the carbon tube or the steel frame? heat, acetone etc?

Cheers Tony
Steve Broad
Steve Broad
Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
Tony Corke - 10/26/2018 11:44:52 AM
Hi,
I want to seperate a fillament wound carbon tube from a steel bicycle frame that was bonded using Vuduglu 
Can this be done without cutting the tube or damaging the carbon tube or the steel frame? heat, acetone etc?

Cheers Tony

Googling this brings up many solvents, but readily available acetone is frequently mentioned. Try it on a test piece first.

Edited 7 Years Ago by Steve Broad
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Unfortunately no off the shelf solvents will touch cured adhesive. Also The bond strength is typically higher than the interlaminar sheer strength of carbon fibre so ripping it apart is likely to lead to the carbon delaminating before the glue goes. If you have a reasonable bond gap, abrading away the adhesive is likely the best way.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
f1rob
f1rob
Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)
Group: Forum Members
Posts: 237, Visits: 4.8K
The best way is heat and movement.
If you can apply the heat to the inside of the meal tube so it transfers outwards to the glue before the carbon even better