If you haven't already done so then i would recommend watching our video series on making a bonnet. It covers exactly what you are doing.
If the frame is reasonably stiff, then use only one layer of cloth on the surface so that your bonnet skin has a balance laminate and is less likely to warp. Probably unlikely to be a major issue but on a good sized bonnet, you could knock things out a few mm with warpage from an unbalanced laminate. Usually that is within tolerance of adjustment on the latch and hinges though.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|