By KP - 7/20/2018 3:02:24 AM
Hi.
Ok happened my fault. I did not steer resin enough or used wrong ratio, after 5 days still have few soft spots on my part. What can I do to fix it? Or it cannot be fixed and i have to scrap the part. Part das not need to look nice it is bottom part of my bonnet.
|
By Warren (Staff) - 7/20/2018 4:01:35 PM
If you haven't already done so then i would recommend watching our video series on making a bonnet. It covers exactly what you are doing.
If the frame is reasonably stiff, then use only one layer of cloth on the surface so that your bonnet skin has a balance laminate and is less likely to warp. Probably unlikely to be a major issue but on a good sized bonnet, you could knock things out a few mm with warpage from an unbalanced laminate. Usually that is within tolerance of adjustment on the latch and hinges though.
|
|