Hi

How You archive matte or satin finish to mould? Using Vinylester/polyester Tooling Gel.

Sanding wet or dry doesn't work, it leaves visible marks.
I've tried also sand/glass blasting, small parts can be ok , but on larger gives me bad blasting stipes/marks. Suggestions?
Is there some chemical?

What is your trick?
Edited 7 Years Ago by FiveO
Reply
FiveO
F
Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)
Group: Forum Members
Posts: 12, Visits: 30
@ Hanaldo
Yes, but my moulds are for solid surface, that's the point why I can't use matte additive.
Edited 7 Years Ago by FiveO
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search