By FiveO - 7/15/2018 4:45:56 PM
Hi
How You archive matte or satin finish to mould? Using Vinylester/polyester Tooling Gel.
Sanding wet or dry doesn't work, it leaves visible marks. I've tried also sand/glass blasting, small parts can be ok , but on larger gives me bad blasting stipes/marks. Suggestions? Is there some chemical?
What is your trick?
|
By FiveO - 7/16/2018 5:23:07 AM
@ Hanaldo Yes, but my moulds are for solid surface, that's the point why I can't use matte additive.
|
|