Hi

How You archive matte or satin finish to mould? Using Vinylester/polyester Tooling Gel.

Sanding wet or dry doesn't work, it leaves visible marks.
I've tried also sand/glass blasting, small parts can be ok , but on larger gives me bad blasting stipes/marks. Suggestions?
Is there some chemical?

What is your trick?
Edited 7 Years Ago by FiveO
Steve Broad
Steve Broad
Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
FiveO - 7/15/2018 4:45:56 PM
Hi

How You archive matte or satin finish to mould? Using Vinylester/polyester Tooling Gel.

Sanding wet or dry doesn't work, it leaves visible marks.
I've tried also sand/glass blasting, small parts can be ok , but on larger gives me bad blasting stipes/marks. Suggestions?
Is there some chemical?

What is your trick?

If the pattern is matte then the mould will be matte :-)

Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Yeh as Steve alluded to, the best way to get a matte finish on your mould is to have a matte finish on the pattern. Sanding doesn't give the same effect as you have discovered, so the best way is to use a matte additive in your 2k clear coat when your spray your pattern. Then you want to be careful when applying your release agent etc so that you don't buff up the matte finish and leave it looking uneven.
FiveO
F
Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)
Group: Forum Members
Posts: 12, Visits: 30
@ Hanaldo
Yes, but my moulds are for solid surface, that's the point why I can't use matte additive.
Edited 7 Years Ago by FiveO
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search