Hi

How You archive matte or satin finish to mould? Using Vinylester/polyester Tooling Gel.

Sanding wet or dry doesn't work, it leaves visible marks.
I've tried also sand/glass blasting, small parts can be ok , but on larger gives me bad blasting stipes/marks. Suggestions?
Is there some chemical?

What is your trick?
Edited 7 Years Ago by FiveO
Reply
Steve Broad
Steve Broad
Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
FiveO - 7/15/2018 4:45:56 PM
Hi

How You archive matte or satin finish to mould? Using Vinylester/polyester Tooling Gel.

Sanding wet or dry doesn't work, it leaves visible marks.
I've tried also sand/glass blasting, small parts can be ok , but on larger gives me bad blasting stipes/marks. Suggestions?
Is there some chemical?

What is your trick?

If the pattern is matte then the mould will be matte :-)