Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
This is a characteristic of honeycombs in general. If you were bonding it and holding it in place using a vacuum bag then you would probably be ok. Aluminium honeycomb may be easier to use on a curve as you can take the curve out by very slight compressing of the cells around the curve.