Bending Nomex honeycomb
http://www.talkcomposites.com/Topic25589.aspx
By mnik
-
4/4/2018 10:25:42 AM
Hello,
I recently purchased a panel of your 4.8 mm Nomex honeycomb, thickness 10 mm. I have a project where I need to bend a strip of the honeycomb about 5 cm wide into a cylinder and glue it on the inside of a tube with a radius of 100 mm. What happens is that the honeycomb gets warped (picture attached) and I could only glue it on the edges. Does anybody have any advice how to solve that? Is this a characteristic of this particular honeycomb or do all behave like that?
By Rosta Spicl
-
10/8/2020 7:17:48 AM
+
x
Warren (Staff) - 10/7/2020 2:49:21 PM
It quite works on mild flat panel. If the shape is more complex, you have to fix the core in correct position over the vacuum bag during vacuuming. That's a nightmare work...