Hello,

I recently purchased a panel of your 4.8 mm Nomex honeycomb, thickness 10 mm. I have a project where I need to bend a strip of the honeycomb about 5 cm wide into a cylinder and glue it on the inside of a tube with a radius of 100 mm. What happens is that the honeycomb gets warped (picture attached) and I could only glue it on the edges. Does anybody have any advice how to solve that? Is this a characteristic of this particular honeycomb or do all behave like that?