Hello!

I am making a rather complex model where making a mould is extremely difficult, and not necessary because it is a one time only. 
There fore, I wonder if it is possible to make the the core out of some kind of polyurethane, and proceed to wrap it in pre-preg and then cure it as usual? Does anyone have any experience on this topic? 
Would the polyurethane handle the heat?
Would it bend or deform under vacuum? (The construction is about 40mm wide at thinnest and about 600mm long)

Best Regards, 
Anders
Replies
Tony2125
Tony2125
Supreme Being (131 reputation)Supreme Being (131 reputation)Supreme Being (131 reputation)Supreme Being (131 reputation)Supreme Being (131 reputation)Supreme Being (131 reputation)Supreme Being (131 reputation)Supreme Being (131 reputation)Supreme Being (131 reputation)
Group: Forum Members
Posts: 12, Visits: 59
Steve Broad
Steve Broad
Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
Tony2125 - 4/1/2018 8:31:40 PM

Interesting site, bookmarked :-)

Tony2125
Tony2125
Supreme Being (131 reputation)Supreme Being (131 reputation)Supreme Being (131 reputation)Supreme Being (131 reputation)Supreme Being (131 reputation)Supreme Being (131 reputation)Supreme Being (131 reputation)Supreme Being (131 reputation)Supreme Being (131 reputation)
Group: Forum Members
Posts: 12, Visits: 59
Yes
I ve looking for foam core solution for a project.
I know some guys use EPS polystyrene, but I don’t know if this require a preparation for using it with preg
What I found was
Rohacell
Soluble foam core from http://www.acmtucson.com/
sold by aeroconsultant.ch
Expandable foam core from https://www.tencatecomposites.com/products/adhesives-and-core
Epoxy foam for Sicomin http://www.sicomin.com/datasheets/product-pdf_fr19.pdf
I will give a try with the last one available in small qty and relatively cheep

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
AndersES - 7 Years Ago
Hanaldo - 7 Years Ago
AndersES - 7 Years Ago
Warren (Staff) - 7 Years Ago
AndersES - 7 Years Ago
scottracing - 7 Years Ago
Hanaldo - 7 Years Ago
Tony2125 - 7 Years Ago
                 Interesting site, bookmarked :-)
Steve Broad - 7 Years Ago
Tony2125 - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search