Yes
I ve looking for foam core solution for a project.
I know some guys use EPS polystyrene, but I don’t know if this require a preparation for using it with preg
What I found was
Rohacell
Soluble foam core from http://www.acmtucson.com/
sold by aeroconsultant.ch
Expandable foam core from https://www.tencatecomposites.com/products/adhesives-and-core
Epoxy foam for Sicomin http://www.sicomin.com/datasheets/product-pdf_fr19.pdf
I will give a try with the last one available in small qty and relatively cheep

Steve Broad
Steve Broad
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
Tony2125 - 4/1/2018 8:31:40 PM

Interesting site, bookmarked :-)

Tony2125
Tony2125
Supreme Being (221 reputation)Supreme Being (221 reputation)Supreme Being (221 reputation)Supreme Being (221 reputation)Supreme Being (221 reputation)Supreme Being (221 reputation)Supreme Being (221 reputation)Supreme Being (221 reputation)Supreme Being (221 reputation)
Group: Forum Members
Posts: 12, Visits: 59
Hanaldo
Hanaldo
Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Tooling board would work, but it wouldn't be lightweight at all, especially the EB700 tooling board as it is a 700kg/M3 density - extremely heavy for use in a final component. You ideally want something no heavier than a 90-100kg/M3 density, but can also take high temperatures without inhibition... There aren't many options that spring to mind for me, but I would suggest it will be an aerospace product. 

As Scott suggested, pre-preg may not be the most suitable choice for this one?
Edited 7 Years Ago by Warren (Staff)
scottracing
scottracing
Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
it would help if you can explain a bit more about what you are trying to achieve? Does it need to be prepreg that you are using? Could you make the core from a cheaper foam material and then skin it using dry fibre and the XCR resin system?

Im doing some work on using 3d printed parts as the sacrificial core but the PLA material isnt able to cope with even a 65degree cure. I would have a look into other materials as the guys above say the PU block will inhibit the cure


AndersES
A
Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)
Group: Forum Members
Posts: 3, Visits: 20
Warren (Staff) - 3/13/2018 2:42:31 PM
PU will inhibit the cure even at relatively low temperatures.  By far the better choice would be an Epoxy Tooling block such as our EP700
Thank you!

Is there any cheaper options on the market?

Warren (Staff)
Warren (Staff)
Supreme Being (36K reputation)Supreme Being (36K reputation)Supreme Being (36K reputation)Supreme Being (36K reputation)Supreme Being (36K reputation)Supreme Being (36K reputation)Supreme Being (36K reputation)Supreme Being (36K reputation)Supreme Being (36K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
PU will inhibit the cure even at relatively low temperatures.  By far the better choice would be an Epoxy Tooling block such as our EB700


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Edited 7 Years Ago by Warren (Staff)
AndersES
A
Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)
Group: Forum Members
Posts: 3, Visits: 20
Hanaldo - 3/12/2018 10:52:04 PM
Polyurethanes will inhibit the cure of epoxies at high temperatures unfortunately. 

Thank you for your answer - but the heat in this case would not be higher than 90-100 degrees celsius. Is this still too high?
If it is, do you have any suggestions or recommendations on what I should use instead?
Maybe the EB700 High Temperature Epoxy Tooling Board would work for example?
- A

Edited 7 Years Ago by Warren (Staff)
Hanaldo
Hanaldo
Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Polyurethanes will inhibit the cure of epoxies at high temperatures unfortunately. 
AndersES
A
Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)
Group: Forum Members
Posts: 3, Visits: 20
Hello!

I am making a rather complex model where making a mould is extremely difficult, and not necessary because it is a one time only. 
There fore, I wonder if it is possible to make the the core out of some kind of polyurethane, and proceed to wrap it in pre-preg and then cure it as usual? Does anyone have any experience on this topic? 
Would the polyurethane handle the heat?
Would it bend or deform under vacuum? (The construction is about 40mm wide at thinnest and about 600mm long)

Best Regards, 
Anders
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search