Hello!

I am making a rather complex model where making a mould is extremely difficult, and not necessary because it is a one time only. 
There fore, I wonder if it is possible to make the the core out of some kind of polyurethane, and proceed to wrap it in pre-preg and then cure it as usual? Does anyone have any experience on this topic? 
Would the polyurethane handle the heat?
Would it bend or deform under vacuum? (The construction is about 40mm wide at thinnest and about 600mm long)

Best Regards, 
Anders
Replies
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Polyurethanes will inhibit the cure of epoxies at high temperatures unfortunately. 
AndersES
A
Forum Member (32 reputation)Forum Member (32 reputation)Forum Member (32 reputation)Forum Member (32 reputation)Forum Member (32 reputation)Forum Member (32 reputation)Forum Member (32 reputation)Forum Member (32 reputation)Forum Member (32 reputation)
Group: Forum Members
Posts: 3, Visits: 20
Hanaldo - 3/12/2018 10:52:04 PM
Polyurethanes will inhibit the cure of epoxies at high temperatures unfortunately. 

Thank you for your answer - but the heat in this case would not be higher than 90-100 degrees celsius. Is this still too high?
If it is, do you have any suggestions or recommendations on what I should use instead?
Maybe the EB700 High Temperature Epoxy Tooling Board would work for example?
- A

Edited 6 Years Ago by Warren (Staff)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
AndersES - 7 Years Ago
Hanaldo - 7 Years Ago
AndersES - 7 Years Ago
Warren (Staff) - 7 Years Ago
AndersES - 7 Years Ago
scottracing - 7 Years Ago
Hanaldo - 7 Years Ago
Tony2125 - 7 Years Ago
                 Interesting site, bookmarked :-)
Steve Broad - 7 Years Ago
Tony2125 - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search