Hello everyone! 

I'm planing on making an intake plenum from carbon fiber and kevlar. It is for a turbocharged car, so it needs to withstand some pressure!
The boost will be under 1 bar at the moment but I'm planning on testing the part on 3 bars at least, for reassurance.
The parts will be made from heat resistant Vinylester probably, if not Epoxy resin and vacuum infusion.

I'm planning on using 3 layers of 200gr 2X2 Twill Carbon fiber and 2 or 3 layers of hybrid 164gr Plain Carbon/Kevlar, alternatly in the layers.
By that, I mean, the first layer will be Carbon fiber, then Carbon/Kevlar, then Carbon fiber etc etc.

Will these layers and fabrics will be enough? Should I add anything or change any of the layers?

Here is the 3D model of the parts in assembly. 

http://www.talkcomposites.com/Uploads/Images/ebdd8fd4-90c6-48d1-b1f0-a5c4.JPG


http://www.talkcomposites.com/Uploads/Images/a0ec41ec-9a6e-4ba7-b162-d36f.JPG
Reply
Elias_GR
Elias_GR
Supreme Being (121 reputation)Supreme Being (121 reputation)Supreme Being (121 reputation)Supreme Being (121 reputation)Supreme Being (121 reputation)Supreme Being (121 reputation)Supreme Being (121 reputation)Supreme Being (121 reputation)Supreme Being (121 reputation)
Group: Forum Members
Posts: 11, Visits: 604
I was thinking exactly the same thing yesterday, about the heat reflective materials.
The one problem is that I don't want to cover the carbon fiber, for aesthetic reasons. The other thing is that I'm thinking that it won't be necessary though cause the engine is a simple inline 4 motor. That means that it has the intake on one side and the exhaust on the exact opposite. The temperature in the intake side will be under 90-100 degrees(Celcius) for sure. 

I guess I'll find it out if everything melts in there! Tongue
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Elias_GR - 9 Years Ago
Hanaldo - 9 Years Ago
Elias_GR - 9 Years Ago
Hanaldo - 9 Years Ago
andygtt - 8 Years Ago
andygtt - 8 Years Ago
Elias_GR - 8 Years Ago
davro - 8 Years Ago
Elias_GR - 8 Years Ago
Jadleybray - 8 Years Ago
Hanaldo - 8 Years Ago
Elias_GR - 8 Years Ago
andygtt - 8 Years Ago
Elias_GR - 7 Years Ago
Hanaldo - 7 Years Ago
Elias_GR - 7 Years Ago
Hanaldo - 7 Years Ago
Elias_GR - 7 Years Ago
ArturK - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search