Carbon fiber intake plenum


Author
Message
ArturK
ArturK
Supreme Being (271 reputation)Supreme Being (271 reputation)Supreme Being (271 reputation)Supreme Being (271 reputation)Supreme Being (271 reputation)Supreme Being (271 reputation)Supreme Being (271 reputation)Supreme Being (271 reputation)Supreme Being (271 reputation)
Group: Forum Members
Posts: 19, Visits: 53
Nice project, I am waiting for more photos.
1.5-2 mm will be quite enought for the wall thickness.


Carbon fiber sheets and composites .
www.dexcraft.com
Elias_GR
Elias_GR
Supreme Being (239 reputation)Supreme Being (239 reputation)Supreme Being (239 reputation)Supreme Being (239 reputation)Supreme Being (239 reputation)Supreme Being (239 reputation)Supreme Being (239 reputation)Supreme Being (239 reputation)Supreme Being (239 reputation)
Group: Forum Members
Posts: 11, Visits: 604
Hanaldo this will be tested on my ''lab rat'' which is a GA series motor that I've boosted a couple of years ago.

Very helpful thread for the oven! Thanks!

A bit more progress now.
I sealed the MDF with automotive primer, sand them and paint them gloss black so i can spot any defects on the surface.
A bit of polishing, some release wax and gelcoat. 
Hopefully, tommorow they will be ready.












Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Interesting... CA, SR? Or something less mainstream? 

The build thread for my oven is herehttp://www.talkcomposites.com/21047/MDF-Curing-Oven?PageIndex=1 

Still working like a charm, and I'm currently considering building a second, bigger version now that I am very active with pre-preg. Definitely the way to go!
Elias_GR
Elias_GR
Supreme Being (239 reputation)Supreme Being (239 reputation)Supreme Being (239 reputation)Supreme Being (239 reputation)Supreme Being (239 reputation)Supreme Being (239 reputation)Supreme Being (239 reputation)Supreme Being (239 reputation)Supreme Being (239 reputation)
Group: Forum Members
Posts: 11, Visits: 604
Hanaldo - 3/16/2018 4:40:00 AM
Good stuff mate, man CNC's make this game too easy! Haha.

Interesting plenum design, I hadn't realised from your drawing it was such a tight area at the back. what sort of engine is it for?

Thanks Hanaldo!
CNC's are really an enormous help!

The intake will be put in a small Nissan engine, for some tests and the we will upscale it for (hopefully) something better.

Also if anyone has made a composite oven, I'd love to learn more information about it because I'm thinking to use pre-preg for the final part.

Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Good stuff mate, man CNC's make this game too easy! Haha.

Interesting plenum design, I hadn't realised from your drawing it was such a tight area at the back. what sort of engine is it for?
Elias_GR
Elias_GR
Supreme Being (239 reputation)Supreme Being (239 reputation)Supreme Being (239 reputation)Supreme Being (239 reputation)Supreme Being (239 reputation)Supreme Being (239 reputation)Supreme Being (239 reputation)Supreme Being (239 reputation)Supreme Being (239 reputation)
Group: Forum Members
Posts: 11, Visits: 604
So after quiet a while I found some time to continue the project!
Yesterday i got the plugs from the CNC and I've already started to seal the wood so I can produce a mold.
I'll get back with plenty of photos from all the steps/


Here are a couple of photos!


Jadleybray
Jadleybray
Supreme Being (222 reputation)Supreme Being (222 reputation)Supreme Being (222 reputation)Supreme Being (222 reputation)Supreme Being (222 reputation)Supreme Being (222 reputation)Supreme Being (222 reputation)Supreme Being (222 reputation)Supreme Being (222 reputation)
Group: Forum Members
Posts: 10, Visits: 85
davro - 1/24/2017 4:18:38 PM
I'm in the same boat I want to create a plenum fairly soon but I don't have access to a prepreg setup oven etc, only an infusion setup.
You could cover some of the areas exposed to heat with a heat reflective materials.

Looking forward to updates Smile

Bit of an older post, however I could use some suggestions in materials for heat reflection.  Suggestions appreciated.  

andygtt
andygtt
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Forum Members
Posts: 157, Visits: 1.2K
I built myself an oven purely so I could make the plenum in prepreg, it was my first ever part in pre preg.

Oven cost around £100-150 to build and around 15hrs.... worth it as I now post cute all my resin infusion parts as well.

My oven is modular in design as I made the walls in 100mm  cellutex and built the heating element and fan into a self made steel unit that I bolt into a cut out in the cellutex.... door is simply one of the sides that I push in and pull out and is just a push fit nothing flash.
Hold temps very well, even overnight after it's turned off.

I made it modular so I could easily change the size and shape of it, this one is only 900x900x800mm so I can't fit in my large rear spoiler hence I've built a coffin shaped over is same materials so I can cure the spoilers.
Elias_GR
Elias_GR
Supreme Being (239 reputation)Supreme Being (239 reputation)Supreme Being (239 reputation)Supreme Being (239 reputation)Supreme Being (239 reputation)Supreme Being (239 reputation)Supreme Being (239 reputation)Supreme Being (239 reputation)Supreme Being (239 reputation)
Group: Forum Members
Posts: 11, Visits: 604
Hanaldo thanks for the reply! 
The resin I'm going to use has 123C Tg, so the only thing "I'm most afraid" is the print through, as you mentioned, but I also can live with it.

On the side where the throttle body flange will sit, I'll have fabricated an aluminum piece that the throttle body will screw on it. 
What can i use to have this aluminum piece glued together with the rest of the carbon fiber plenum?
Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
You really should be ok, you may just suffer a bit of print-through. I've made plenty of engine bay parts (including plenums) using an infusion resin with a Tg of 90, and for the most part they haven't even printed too badly. Hell, I've made inner guards for a 1500hp twin-turbo Impala, where the inner guards sit 5mm away from the exhaust manifold. These would easily be exposed to over 350C. Yes, they are discoloured quite badly in the area they sit close to the manifold, but that is the worst of it. 



I mean I'm not necessarily recommending using a 90 Tg resin for a 350C application, rather just pointing out that your parts aren't going to melt and fall apart. What will happen is that if they are exposed to heat above their capabilities then the resin will soften a touch, which will certainly lead to print through. If the parts are under load and are unsupported, they may distort quite badly depending on their geometry and the degree of load etc. For example on something like a plenum, if you had a hose clamp on the inlet piping, this may distort the mouth of the plenum. Or if you had your intake piping bolted onto a throttle body, and this was unsupported weight that was 'hanging' off the front of the plenum, then this may distort the entire plenum. 

So things like that are what you will want to consider. Otherwise, if you are only going 15-20 degrees above their Tg, the worst you are likely to experience is a bit of discolouration and some print-through. 
Edited 9 Years Ago by Hanaldo