Author
Message
Elias_GR
Elias_GR
Supreme Being (121 reputation)Supreme Being (121 reputation)Supreme Being (121 reputation)Supreme Being (121 reputation)Supreme Being (121 reputation)Supreme Being (121 reputation)Supreme Being (121 reputation)Supreme Being (121 reputation)Supreme Being (121 reputation)
Group: Forum Members
Posts: 11, Visits: 604
Hello everyone! 

I'm planing on making an intake plenum from carbon fiber and kevlar. It is for a turbocharged car, so it needs to withstand some pressure!
The boost will be under 1 bar at the moment but I'm planning on testing the part on 3 bars at least, for reassurance.
The parts will be made from heat resistant Vinylester probably, if not Epoxy resin and vacuum infusion.

I'm planning on using 3 layers of 200gr 2X2 Twill Carbon fiber and 2 or 3 layers of hybrid 164gr Plain Carbon/Kevlar, alternatly in the layers.
By that, I mean, the first layer will be Carbon fiber, then Carbon/Kevlar, then Carbon fiber etc etc.

Will these layers and fabrics will be enough? Should I add anything or change any of the layers?

Here is the 3D model of the parts in assembly. 

http://www.talkcomposites.com/Uploads/Images/ebdd8fd4-90c6-48d1-b1f0-a5c4.JPG


http://www.talkcomposites.com/Uploads/Images/a0ec41ec-9a6e-4ba7-b162-d36f.JPG
Reply
andygtt
andygtt
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 157, Visits: 1.2K
I made a carbon plenum for my noble over the past 8 months... not bonded it together but its strong enough to stand on so is easily as strong as the stock plastic one was.

Made it in pre reg, 1 layer finish, 3 layers of 450... however the shape adds a lot to the rigidity, if i had flat surfaces like yours i would have beefed that up considerably.





GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Elias_GR - 9 Years Ago
Hanaldo - 9 Years Ago
Elias_GR - 9 Years Ago
Hanaldo - 9 Years Ago
andygtt - 8 Years Ago
andygtt - 8 Years Ago
Elias_GR - 8 Years Ago
davro - 8 Years Ago
Elias_GR - 8 Years Ago
Jadleybray - 8 Years Ago
Hanaldo - 8 Years Ago
Elias_GR - 8 Years Ago
andygtt - 8 Years Ago
Elias_GR - 7 Years Ago
Hanaldo - 7 Years Ago
Elias_GR - 7 Years Ago
Hanaldo - 7 Years Ago
Elias_GR - 7 Years Ago
ArturK - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search