Good morning

I am making am mould for a bonnet scoop with the intentions at this stage to wet lay up only with our bagging or vacuum and wonder if :-

Can I wet lay up one ply of 200gsm 2x2 twill carbon only and let that cure off to aid getting a good finish (Prevent bridging and dry spots) and then lay up further plies for strength afterwards.

I will be using Easy Composites EL2 Epoxy Laminating Resin with fast and slow hardeners

Regards

Ian
Reply
George Sychrovsky
George Sychrovsky
Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)
Group: Forum Members
Posts: 24, Visits: 1.6K
On my clear carbon finished parts I do a single ply first let it cure until it will not get disturb by subsequent plies , mainly it helps eliminating pinholes and bubbles,


---------------------------------------------------------------------
Disclaimer opinions of others will vary depending on what they are selling