This shape part would be really to make in polyester resin.

One layer of your carbon twill well done and just a couple more of a chop strand mat straight on the back.




George Sychrovsky
George Sychrovsky
Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)
Group: Forum Members
Posts: 24, Visits: 1.6K
On my clear carbon finished parts I do a single ply first let it cure until it will not get disturb by subsequent plies , mainly it helps eliminating pinholes and bubbles,


---------------------------------------------------------------------
Disclaimer opinions of others will vary depending on what they are selling
Porkster0
Porkster0
Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)
Group: Forum Members
Posts: 14, Visits: 69
Hi Hanaldo

Thanks for the reply, I was of thinking of do one ply only and letting it cure first

as I am concerned that it will be difficult to get the profile/shape at the front of the scoop mould good enough with all the multiple plies(4-5) with our it pulling away from the mould and causing bridging dry spots as I don't have any vacuum kit

Regards

Ian
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
You can. But why would you want to? Multiple layers don't contribute to surface finish. 
Porkster0
Porkster0
Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)
Group: Forum Members
Posts: 14, Visits: 69
Good morning

I am making am mould for a bonnet scoop with the intentions at this stage to wet lay up only with our bagging or vacuum and wonder if :-

Can I wet lay up one ply of 200gsm 2x2 twill carbon only and let that cure off to aid getting a good finish (Prevent bridging and dry spots) and then lay up further plies for strength afterwards.

I will be using Easy Composites EL2 Epoxy Laminating Resin with fast and slow hardeners

Regards

Ian
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search