I am making am mould for a bonnet scoop with the intentions at this stage to wet lay up only with our bagging or vacuum and wonder if :-
Can I wet lay up one ply of 200gsm 2x2 twill carbon only and let that cure off to aid getting a good finish (Prevent bridging and dry spots) and then lay up further plies for strength afterwards.
I will be using Easy Composites EL2 Epoxy Laminating Resin with fast and slow hardeners
Regards