Group: Moderators
Posts: 226,
Visits: 334
|
Hanaldo is speaking as someone with expert knowledge and a lot of skill in mould making, forgive me mate
but
if you have limited experience of plugs and moulds you will find it hard to do as one, get the edge angles right and it will work but wrong and that thing will be locked, you may find it easier to split it down the middle.
|